  Main parameters
nd = 1.658441
ne = 1.661520
Vd = 50.89
Ve = 50.60
nF - nC = 0.012937
nF' - nC' = 0.013072
Coloring:
0.366 - 0.331 mkm.

  Coefficients of dispertion formulas
Type: Schott
Spectral range: 0.4046561 - 0.76819 mkm.
C1 = 2.69603796 C2 = -0.0100729839 C3 = 0.0188657945 C4 = 0.00036803849 C5 = 0.00000406084448 C6 = 0.000000457460676

  Refraction index
n 2.3254-----
n 1.9701-----
n 1.5296-----
n 1.06-----
n t-----
n s-----
n r1.652368
n C1.654554
n C'1.655169
n 0.63281.655745
n D1.658326
n d1.658441
n e1.661520
n F1.667492
n F'1.668241
n g1.674690
n h1.680740
n i-----
n 0.3341-----
n 0.3126-----
n 0.2967-----
n 0.2804-----
n 0.2483-----
  Relative partial dispertion
PC,t-----
PC,A'0.3369
Pd,C0.3003
Pe,C0.5384
Pg,d1.2559
Pg,F0.5563
Ph,g0.4676
Pi,g-----
PC',t-----
Pe,C'0.4908
PF',e0.5195
Pi,F'-----
 transmittance: 10 mm
τ0.340.08
τ0.350.37
τ0.360.66
τ0.370.83
τ0.380.911
τ0.390.951
τ0.40.972
τ0.420.988
τ0.440.992
τ0.460.995
τ0.480.998
τ0.50.999
τ0.550.999
τ0.60.999
τ0.650.999
τ0.70.999
τ0.80.999
τ0.90.999
τ10.999
τ1.20.999
τ1.40.999
τ1.60.999
τ1.80.99
τ20.981
τ2.20.941
τ2.40.85

  mechanical
Knoop hardness: 521
Abrasion: 184

  Chemical
Resistance to acids: 3

 Temperature coefficient of linear expansion
Temp. range, CValue, 1/C*10^-7
100 ~ 30082